Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 76.0 - 77.0 MPa | 11000 - 11200 psi | Average value: 76.3 MPa Grade Count:3 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Compressive Yield Strength | >= 76.0 MPa | >= 11000 psi | Superior Quality |
Kazanorgsintez PC-005 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Compressive Yield Strength | >= 76.0 MPa | >= 11000 psi | Superior Quality |
Kazanorgsintez PC-010 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of die-casting.Information Provided by Kazanorgsintez |
|||
Compressive Yield Strength | 76.0 MPa | 11000 psi | ASTM D695 |
Adell AI-10 Nylon 66, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 76.0 MPa | 11000 psi | ASTM D695 |
Ashley Polymers Ashlene® 1041R Polycarbonate A general purpose, injection molding grade, natural resin.Data provided by the manufacturer |
|||
Compressive Yield Strength | 76.0 MPa | 11000 psi | ASTM D695 |
Ashley Polymers Ashlene® 1061R Polycarbonate A general purpose polycarbonate, low melt flow for injection molding.Data provided by the manufacturer |
|||
Compressive Yield Strength | 76.0 - 86.2 MPa | 11000 - 12500 psi | Average value: 82.8 MPa Grade Count:9 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Compressive Yield Strength | 76.0 MPa | 11000 psi | ASTM D695 |
Adell AI-30 Nylon 66, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 76.0 MPa | 11000 psi | ASTM D695 |
Ashley Polymers Ashlene® P1021R Polycarbonate A prime general purpose injection molding grade, natural resin with easy mold release.Data provided by the manufacturer |