Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 69.0 MPa | 10000 psi | 7 Day Cure; ASTM D695 |
Protective Coating PC-Concrete™ Epoxy Concrete Anchoring and Repair System PC Concrete™ epoxy gel is an anchoring and concrete repair product. PC Concrete™ is formulated for anchoring threaded rods, bolts, rebar dowels and smooth dowels into concrete, grout filled block,.. |
|||
Compressive Yield Strength | 69.0 - 186 MPa | 10000 - 27000 psi | Average value: 124 MPa Grade Count:5 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Compressive Yield Strength | 69.0 MPa | 10000 psi | 10% compression |
Zircar Refractory Composites RS-A Refractory Sheet ZRCI`s Refractory Sheet Type RS-A Moldable is a tough ceramic fiber reinforced insulation which contains no asbestos. Developed as an asbestos board replacement for induction coil liners and molten .. |
|||
Compressive Yield Strength | 69.0 MPa | 10000 psi | at 2% compression parallel to thickness |
Zircar Refractory Composites RS-100 Refractory Sheet ZIRCAR Refractory Sheet Type RS-100 is a ceramic fiber reinforced structural alumina composite material with useful properties to 1260°C (2300°F). It has exceptional flexural and compressive stren.. |