Mechanical Properties Metric English Comments
Compressive Yield Strength 31.0 - 183 MPa
4500 - 26500 psi
Average value: 108 MPa Grade Count:24
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Compressive Yield Strength 31.0 - 68.9 MPa
4500 - 10000 psi
Average value: 49.6 MPa Grade Count:8
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Compressive Yield Strength 31.0 MPa
4500 psi
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density
Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech..
Compressive Yield Strength 31.0 MPa
4500 psi
ASTM D395
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience ..
Compressive Yield Strength 31.0 MPa
4500 psi
TM R050-38
Resinlab® EP1026HP Epoxy Adhesive
Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan..