Polymer Property : Compressive Yield Strength = 30550 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 210.6 MPa
30550 psi
ASTM D695
Plenco 7300 Phenolic, Nodular, Injection Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..