Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 195 - 225 MPa | 28300 - 32600 psi | Average value: 211 MPa Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Compressive Yield Strength | 195 MPa | 28300 psi | ASTM D695 |
Chevron Phillips Xtel® XK2140 Polyphenylene Sulfide Alloy
(discontinued **) Black Polyphenylene Sulfide AlloyXtel™ XK2140 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties along with .. |