Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 220 MPa
31900 psi
ASTM D695
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade
Amber pelletsInformation provided by Infinite Polymer System II.
Compressive Yield Strength 220 MPa
31900 psi
ASTM D695
Performance Polymers IPS II PPL-C4219 PEKK (Polyetherketoneketone) Linear Wear Grade
Black pellets; Carbon fiber/PTFE/Graphite compoundInformation provided by Infinite Polymer System II.
Compressive Yield Strength 220 MPa
31900 psi
ASTM D695
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy
Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and..