Polymer Property : Compressive Yield Strength = 195 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 195 - 225 MPa
28300 - 32600 psi
Average value: 211 MPa Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Compressive Yield Strength 195 MPa
28300 psi
ASTM D695
Chevron Phillips Xtel® XK2140 Polyphenylene Sulfide Alloy  (discontinued **)
Black Polyphenylene Sulfide AlloyXtel™ XK2140 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties along with ..