Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 151 MPa | 21900 psi | ASTM D695 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Compressive Yield Strength | 151 MPa | 21900 psi | ASTM D695 |
Westlake Plastics Tempalux® Polyetherimide For Medical Applications Medical grade Tempalux is made from Ultem® polyetherimide resin, an amorphous thermoplastic which exhibits excellent resistance to a wide range of chemicals and disinfectants. Ultem maintains its .. |