Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 9.30 MPa | 1350 psi | ASTM D695 |
3M Dyneon™ CC085 PTFE, PPS-Filled
(discontinued **) Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon. |
|||
Compressive Yield Strength | >= 9.31 MPa | >= 1350 psi | Bare, min |
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Compressive Yield Strength | 9.31 MPa | 1350 psi | Bare, typ |
Hexcel® HexWeb® HRP - 3/16 - 8.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |