Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Graves Tear Strength = 856 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 150 kN/m
856 pli
ASTM D1004
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer
WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look ..
Graves Tear Strength 150 kN/m
856 pli
without nick; ISO 34
DSM Arnitel® PL650 Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Graves Tear Strength 150 kN/m
856 pli
without nick; ISO 34
DSM Arnitel® PL650 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Graves Tear Strength 150 kN/m
856 pli
UV Postcure; ASTM D1004-09
DSM Somos® BioClear
Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w..
Copyright © lookpolymers.com All Rights Reserved