Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 115 kN/m | 656 pli | without nick; ISO 34 |
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Graves Tear Strength | 115 kN/m | 656 pli | without nick; ISO 34 |
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |