Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 60.0 kN/m | 342 pli | without nick; ISO 34 |
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Graves Tear Strength | 60.0 kN/m | 342 pli | without nick; ISO 34 |
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Graves Tear Strength | 60.0 kN/m | 342 pli | without nick; ISO 34 |
DSM Arnitel® EM400 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Graves Tear Strength | 60.0 - 150 kN/m | 342 - 856 pli | Average value: 92.5 kN/m Grade Count:6 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Graves Tear Strength | 60.0 kN/m | 342 pli | without nick; ISO 34 |
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |