Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 35.0 kN/m | 200 pli | TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber