Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 67.7 MPa | 9820 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0951 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 67.7 MPa | 9820 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0951 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |