Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Total 819E Polystyrene
(discontinued **) Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Polymer Resources NY66-IM2 Impact Modified Nylon 66 Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are .. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-10GB/15KV Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledAramid Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
PolyOne Edgetek® AT-20GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (Cond)
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 FR IM HS BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Techmer ES HiFill FR® PBT/ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Techmer ES Luriblend® PA4/6 TL15 HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized, Low Friction, Good Wear Resistance and LubricatedInformation provided by TP Com.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Techmer ES HiFill® HDPE GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ecomass® 1080BI64 Filled Polyamide Nontoxic alternative compound for weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Technical Po.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | Cross; IPC TM-650 2.4.4 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Cast Nylons Nycast® 12 Cast Nylon 12 NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical chara.. |
|||
Flexural Strength | 62.1 - 82.7 MPa | 9000 - 12000 psi | |
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC. |