Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D-790 |
Plaskolite Optix® CA - 1000 I High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D-790 |
Plaskolite Optix® CP - 1000 I High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D-790 |
Plaskolite Optix® CP - 1000 IG High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D-790 |
Plaskolite West Optix® CA - 1000 I High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D-790 |
Plaskolite West Optix® CP - 1000 IG High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D790 |
Oxford Polymers INJ-FR Glass Fiber Reinforced ABS, Flame Retardant Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® FRA204 ABS High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D790 |
Chase Plastics CP Pryme® A100HH ABS Features: High heat resistanceForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D790 |
Chase Plastics CP Pryme® N100STL (DAM) Nylon 6, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | Cross; IPC TM-650 2.4.4 |
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran.. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | |
BCC Products BC 6060 Epoxy Surface Coat/Casting BC 6060 is a blue epoxy, abrasion resistant surfacing resin. Commonly referred to as “die surface” material, this system may be applied by brush or if preferred, cast in thin sections to a maximum.. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | |
BCC Products BC 6005 Epoxy Surface Coat BC 6005 is a snow white thixotropic epoxy resin designed specifically for quality reproduction of a variety of surfaces. A room temperature cure system that offers ample working time yet affords qui.. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | |
BCC Products BC 7136-2 Epoxy Casting BC7136-2 is an aluminum filled thick section casting system with heat resistance to 300ºF. May be cast to a thickness of 2 inches in non-conductive molds, 3 inches in conductive molds and thicker s.. |
|||
Flexural Strength | 61.4 MPa | 8900 psi | ASTM D-790 |
Plaskolite West Optix® CP - 1000 I High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |