Mechanical Properties Metric English Comments
Flexural Strength 86.7 MPa
12600 psi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne