Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L7005 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon L7005 is recommended for whites and light pastel colors only.Note: Physical properties based on L7005 tan 3210 sample.Information provided by PolyOne |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L7007 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon L7007 is recommended for whites and light pastel colors only.Geon L7007 is a higher gloss version of L7005.Information provided by PolyOne |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Polymer Resources PPX-GP6 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P10017FRMA Polycarbonate Polycarbonate, General Purpose, Flame RetardantInformation provided by Ravago. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Techmer ES HiFill® ABS LG GF10 UV BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerFeatures: Good UV Resistance and Low GlassAppearance: BlackInform.. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Techmer ES Plastiblend® ABS/PA 1700 B1 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Techmer ES Plastiblend® PPS/F 0328 Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Samsung Cheil Industries Infino® PCA-NH1015V Flame Retardant |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Samsung Cheil Industries Infino® PCA-NH1015V Flame Retardant |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Techmer ES Plastiblend® ABS/PA 1700 B2 Availability: North AmericaForms: PelletsAppearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | |
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound Improved Crack Resistance & Bond Strength. High Temperature Resistance, Thermally Conductive, Low Viscosity. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Aremco Aremco-Bond™ 2315 High Performance Epoxide High Temperature, Low Viscosity, Potting Compound for Electrical Applications. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Techmer ES Luriblend® POM CO SL2 MB Acetal Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerTPCI# 9809114Information provided by TP Composites, Inc. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Techmer ES Plastiblend® ABS/PA 1700 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |