Polymer Property : Flexural Strength = 84.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 84.1 MPa
12200 psi
ASTM D790
Ravago Manufacturing Americas Hysun™ A3525 ASA+PC
Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago
Flexural Strength 84.1 MPa
12200 psi
ASTM D790
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid)
Interior application for thick & thin gauge profile application.Information provided by PolyOne
Flexural Strength 84.1 MPa
12200 psi
ASTM D790
PolyOne Lubri-Tech™ AT-15CF/5T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated  (discontinued **)&l
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Strength 84.1 MPa
12200 psi
ASTM D 790
Styrolution PS 3100/3101 GPPS
Good balance of flow and set-up propertiesModerate heat resistanceUSP Class VI certifiedInformation provided by Styrolution
Flexural Strength 84.1 MPa
12200 psi
ASTM D 790
Styrolution PS 3190/3191 GPPS
Low residual styrene monomer contentGood balance of flow and set-up propertiesInformation provided by Styrolution
Flexural Strength 84.1 MPa
12200 psi
ASTM D790
Styron Pulse® 2000 ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Flexural Strength 84.1 MPa
12200 psi
ASTM D790
Ensinger Tecapeek® XP-97 Compression Molded PEEK Compound, 30% Graphite Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Strength 84.1 MPa
12200 psi
ASTM D-790
Axiall 8302 Rigid PVC, Extrusion & Molding
Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such ..
Flexural Strength 84.1 MPa
12200 psi
ASTM D790
Chase Plastics CP Pryme® N213GL (COND, 50% RH) Nylon 6, 13% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Strength 84.1 MPa
12200 psi
ASTM D-790
Axiall 5006 Rigid PVC, Extrusion, Natural
Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf..
Flexural Strength 84.1 MPa
12200 psi
ASTM D-790
Axiall 5006 Rigid PVC, Extrusion, White
Georgia Gulf 5006 White is a rigid PVC pellet compound designed for extrusion of rigid PVC house siding, window profiles and various contours where maximum weather resistance is required. Georgia G..