Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 81.7 MPa | 11800 psi | ASTM D790 |
PolyOne Maxxam™ PPH-20G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 81.7 MPa | 11800 psi | ASTM D790 |
PolyOne Maxxam™ PPH-20G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |