Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Techmer ES HiFill® PA6 0500 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Techmer ES HiFill® PA6 0232 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | 8 lb Core, 6 hrs @ 220°F, Vacuum Bag |
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe.. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D638 |
Plastics Group Polifil® GFRMPPCC-10 10% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Ecomass® 1050ZD96 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and .. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Ecomass® 1080TU95 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Ecomass® 1080TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Ecomass® 1080ZB92 Filled Polyamide Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyExcellent ToughnessInformation provided by Technical Polymers |
|||
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Ecomass® 1080ZD95 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Ecomass® 1080ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Flexural Strength | 49.0 MPa | 7100 psi | |
3M Scotchkote™ RG 501 Urethane Metal Repair Scotchkote Urethane Metal Repair RG 501 has been specifically developed as a rapid curing repair system for rebuilding and repairing equipment requiring good mechanical strength.Product Features:Com.. |