Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 465 MPa | 67400 psi | |
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Flexural Strength | 465 MPa | 67400 psi | |
Lehmann & Voss LUVOCOM® 1104/XCF/30 Polyether ketone, with carbon fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,.. |