Polymer Property : Flexural Strength = 62.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Multibase Nylex™ 4032 Polyamide + PP
Forms: PelletsInformation provided by Multibase
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM)
Information provided by Ravago.
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 401 FR Polystyrene (PS), Glass Fiber - Flame Retardant - UL94
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 499 X 83696 Polystyrene (PS), Glass Fiber - Permanently Anti-static
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 600 FR UV Acrylonitrile Butadiene Styrene (ABS), Flame Retardant - UV Stabilized
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Total 819E Polystyrene  (discontinued **)
Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof..
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Polymer Resources NY66-IM2 Impact Modified Nylon 66
Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are ..
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
PolyOne Edgetek® AT-20GB/000 Acetal-Copolymer, Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Techmer ES HiFill FR® PBT/ABS FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Techmer ES Luriblend® PA4/6 TL15 HS
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized, Low Friction, Good Wear Resistance and LubricatedInformation provided by TP Com..
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company ESD C 480 HI Polystyrene (PS), Impact Modified - Carbon Fiber - ESD Protection - Electrically Conductive
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company PermaStat® 300 Polycarbonate (PC), ESD Protection - Permanently Anti-static - UL94 HB
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 183 TFE 15 Polypropylene (PP), Carbon Fiber - PTFE Lubricated
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 200 D TFE 18 SI 2 Nylon 6/12 (PA), PTFE Lubricated - Silicone Lubricated
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 1300 TFE 10 Polyphenylene Sulfide (PPS), PTFE Lubricated
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 175 X HB Polypropylene (PP), Glass Fiber - Glass Bead - UL94 HB
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 199 X 132495 A Polypropylene (PP), High Flow - Cellulose Fiber - 20% Renewable Resource Content
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 200 H MS 4 Impact-Modified Nylon 6/6 (PA), Molybdenum Disulfide
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 2099 X 124789 D Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 79%Renewable Resource Content
Not optically transparent.  Thick wall sections can be hazy. For detailed processing information, see the PLA Molding Guide on the RTP Company website.
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Ecomass® 1003ZD95 Tungsten Filled COPA
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by..
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Ecomass® 1080BI64 Filled Polyamide
Nontoxic alternative compound for weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Technical Po..
Flexural Strength 62.1 MPa
9000 psi
Cross; IPC TM-650 2.4.4
Arlon CLTE-XT High Precision Ceramic PTFE
Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing ..
Flexural Strength 62.1 - 82.7 MPa
9000 - 12000 psi
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade
BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r..
Flexural Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v..
Flexural Strength >= 62.1 MPa
>= 9000 psi
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System
Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to..
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
PolyOne Lubri-Tech™ AT-25GB/5T-2S Acetal-Copolymer, Glass Bead Filled, PTFE/Silicone Lubricated  (discontinued
Description/Features:Glass Bead FilledPTFE/Silicone LubricatedInformation provided by PolyOne Corporation.
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
PolyOne Stat-Tech™ AT-000/000 ESD Acetal-Copolymer  (discontinued **)
Description/Features:AntistaticInformation provided by PolyOne Corporation.
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 2099 X 137399 A NS Polyester Alloy Flame Retardant - UV Stabilized - Medical Cleaner Resistant - No Subs
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 2099 X 138762 H PC/PBT Alloy Permanently Static Dissipative - ESD Protection - Impact Modified - UV Stabilized
This compound has been formulated to meet the static dissipative requirements of the ATEX Directive.
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
RTP Company RTP 3005 Polymethylpentene (PMP), Glass Fiber