Polymer Property : Flexural Strength = 59500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 410 MPa
59500 psi
Lehmann & Voss LUVOCOM® 21-7979 Polyamide 6/6T, with glass fiber, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.High dimensionally stable prec..
Flexural Strength 410 MPa
59500 psi
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5%
Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture..
Flexural Strength 410 MPa
59500 psi
GBC Grade 99 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
Flexural Strength 410 MPa
59500 psi
Sapco S.SiC Silicon Carbide
Information provided by Sapco.
Flexural Strength 410 MPa
59500 psi
DIN EN 843-1
CeramTec Rocar® S Silicon Carbide, SSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Flexural Strength 410 MPa

@Temperature -40.0 °C
59500 psi

@Temperature -40.0 °F
ASTM Test
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned)
Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio..
Flexural Strength 410 MPa

@Temperature 23.0 °C
59500 psi

@Temperature 73.4 °F
Ceradyne Ceralloy® 546-3E Boron Carbide
Features:low porosityhigh puritysingle phaseApplications:semiconductor componentsInformation provided by Ceradyne Company
Flexural Strength 410 MPa

@Temperature 23.0 °C
59500 psi

@Temperature 73.4 °F
Ceradyne Ceralloy® 546-4E Boron Carbide
Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co..
Flexural Strength 410 MPa

@Temperature 23.0 °C
59500 psi

@Temperature 73.4 °F
Ceradyne Ceralloy® 546 Boron Carbide
Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co..