Mechanical Properties Metric English Comments
Flexural Strength 386 MPa
56000 psi
ASTM D-790
PlastiComp Complet® LCF15/LGF35 – PA66 BLK Polyamide 66, 50% Long Carbon/Glass Fiber
Composite PelletsInformation provided by PlastiComp, Inc.
Flexural Strength 386 MPa
56000 psi
ASTM D790
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Flexural Strength 386 MPa
56000 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA
LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Strength 386 MPa
56000 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific)
LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Strength 386 MPa
56000 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON UV00ASU PPA
LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural.
Flexural Strength 386 MPa
56000 psi
ASTM D790
Applied Composites 175 Vinylester SMC
Industry Application: TransportationProduct Application: Structural ExteriorDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation.
Flexural Strength 386 MPa
56000 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON UV00AS PPA
LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural.