Mechanical Properties Metric English Comments
Flexural Strength 355 MPa
51500 psi
ISO 178
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced  (discontinued **)
GATONE™ PEEK grades with carbon fiber reinforcements ranging from 10- 40 % are available in natural or desired color. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
Flexural Strength 355 MPa
51500 psi
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Flexural Strength 355 MPa
51500 psi
ASTM D790
Solvay TECHNYLSTARâ„¢ AFX 218S V50 PA6, 50% glass filled, DRY
Description: High stiffness materials TECHNYLSTAR Polyamide 66, reinforced with 50% of glass fiber, heat stabilized for injection molding. Characterized by a high fluidity of the melt. Available in:..
Flexural Strength 355 MPa
51500 psi
ISO 178
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber
Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p..
Flexural Strength 355 MPa
51500 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66
LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 355 MPa
51500 psi
ISO 178
Solvay TECHNYL® A 118L V50 PA66, 50% glass fiber, Eh 0
Description: TECHNYL A 118L V50 is a polyamide 6.6 reinforced with 50% of glass fiber, with thermal stability, UV protection and modified viscosity that provides better superficial appearance. Color..
Flexural Strength 355 MPa
51500 psi
ISO 178-93
Wellman Wellamid® GF1750-N1 50% Glass Fiber Reinforced Nylon 6
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Flexural Strength 355 MPa
51500 psi
dry; ISO 178
DSM Novamid® 1013G45 1 NA PA6-GF45
45% Glass Reinforced, Injection Molding
Flexural Strength 355 MPa
51500 psi
dry; ISO 178
DSM Novamid® 1013GH45 1 NA/BK701 PA6-GF45
45% Glass Reinforced, Heat Stabilized, Injection Molding
Flexural Strength 355 MPa
51500 psi
ISO Data
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Dry)
Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil..