Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 3.45 MPa | 500 psi | |
Pyrotek Pyroboard™ S1300 Roller Pyroboard™ S1300 was developed specifically for use in hotter zones of an annealing furnace.Information provided by Pyrotek. |
|||
Flexural Strength | 3.45 MPa | 500 psi | Burst Strength |
Saint-Gobain COHRlastic® 1115 Abrasion Resistant Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Flexural Strength | 3.45 MPa | 500 psi | Burst Strength |
Saint-Gobain COHRlastic® 3016 Low Temperature Flexibility Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Flexural Strength | 3.45 MPa | 500 psi | Burst Strength |
Saint-Gobain COHRlastic® 1015 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Flexural Strength | 3.45 MPa | 500 psi | Diaphragm Burst Strength |
Saint-Gobain COHRlastic® CF4420 High Heat Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Flexural Strength | 3.45 MPa | 500 psi | |
Cotronics Resbond™ 940 High Temperature Ceramic Adhesive, Fast Set |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron Ferrobond-LH™ Steel-Filled, Structural Adhesive Putty; High Temperature Liquid Ferrobond-LH™ is Ferrobond-L™ for up to 320° F (160° C) under stress; Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 23 lbs/gal; B: 9.8 lbs/gal; mixin.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron Ferrobond-L™ Steel-Filled, Structural Adhesive Putty; Liquid Ferrobond-L™ is a fluid pourable Ferrobond-P™. Casting version of Ferrobond-P™. Choose when flowing consistency is needed for pouring. Excellent for tooling. Technical Characteristics: A: 23 lbs.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste Metalfix-PH™ is MetalFix-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical Cha.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron Metalfix-P™ Aluminum-Filled, Structural Adhesive Putty; Paste Metalfix-P™ is an aluminum-filled, structural adhesive putty. Patch, bond, resurface metal, structural components, patterns, molds, pipes, tanks, sculptures, and appliances. Forms a permanent bond .. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste Ferrobond-P™ is a steel-filled, structural adhesive putty. Repair or fill metal components, castings, tanks, and magnetic fixtures. Preferred to Metalfix-P™ where heavier weight, magnetism, or hig.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron Metalfix-LH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Liquid Metalfix-LH™ is MetalFix-L™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 14.8 lbs/gal; B: 9.8 lbs/gal; mixin.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron SS-Bond-PH™ Stainless-Steel-Filled, Structural Adhesive Putty; High Temperature Paste SS-Bond-PH™ is SS-Bond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ra.. |
|||
Flexural Strength | 3.45 - 48.3 MPa | 500 - 7000 psi | |
Abatron Metalfix-L™ Aluminum-Filled, Structural Adhesive Putty; Liquid Metalfix-L™ is a fluid-pourable version of MetalFix-P™. For patterns, molds, prototypes, casting, and all applications where a castable, fluid, MetalFix-P™ is needed. Excellent for tooling. Techn.. |