Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 341 MPa | 49500 psi | ASTM D790 |
PlastiComp Complet® LBF50-PA66 50% Long Basalt Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Flexural Strength | 341 MPa | 49500 psi | ASTM D-790 |
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 50% long glass fiber reinforcementInformation provided by PlastiC.. |
|||
Flexural Strength | 341 MPa | 49500 psi | ASTM D790 |
Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced Nylon 66, 60% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Flexural Strength | 341 MPa | 49500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding. |
|||
Flexural Strength | 341 MPa | 49500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LC008EXP PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LC008EXP is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include Electrically Conductive, Easy Molding. |
|||
Flexural Strength | 341 MPa | 49500 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 341 MPa | 49500 psi | ISO 178 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |