Polymer Property : Flexural Strength = 49000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 338 MPa
49000 psi
ASTM D-790
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Flexural Strength 338 MPa
49000 psi
ASTM D790
Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced
Product Description: Carbon Fiber (20% Reinforced), PEEK, Polyetheretherketone, injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon fiber Special Ch..
Flexural Strength 338 MPa
49000 psi
ASTM D790
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Flexural Strength 338 MPa
49000 psi
ASTM D790
Techmer ES HiFill® HTN GF HS L High Temp Nylon 50% Glass Filled
Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Heat ResistanceInformation provided by TP Composit..
Flexural Strength 338 MPa
49000 psi
ASTM D790
Techmer ES HiFill® PA6 GF60 L BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo..
Flexural Strength 338 MPa
49000 psi
ASTM D790
Techmer ES HiFill® PA6/6 GF40 HS L 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati..
Flexural Strength 338 MPa
49000 psi
ASTM D790
Techmer ES HiFill® PA6/6 GF40 HS L BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N..
Flexural Strength 338 MPa
49000 psi
ASTM D790
Techmer ES HiFill® PA6/6 GF40 UV L BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceAppearan..
Flexural Strength 338 MPa
49000 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA
LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized.
Flexural Strength 338 MPa
49000 psi
ASTM D790
Techmer ES HiFill FR® PA6/6 GF40 FR HS L 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform..
Flexural Strength 338 MPa
49000 psi
ASTM D790
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Flexural Strength 338 MPa
49000 psi
ASTM F417
CoorsTek AD-90 Alumina (nom. 90% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..