Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Multibase Nylex™ 2185 CR Polyamide + PP Forms: PelletsFeatures:Chemical Resistance, GoodInformation provided by Multibase |
|||
Flexural Strength | 49.6 MPa | 7190 psi | ASTM D790 |
PolyOne Maxxam™ DP 4980-1-1000 Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 49.6 MPa @Temperature 100 °C |
7190 psi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Total 965E Polystyrene
(discontinued **) Polystyrene 965E is a high-impact polystyrene. The extruder will see that 965E produces sheet with a dull matte finish and superior wetting tension to meet the printers needs.965E is specially desig.. |
|||
Flexural Strength | 49.6 MPa @Temperature 100 °C |
7190 psi @Temperature 212 °F |
2; ISO 178 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D 790 |
Styrolution PS 6200/6201 HIPS Excellent toughnessDesigned for deep draw thermoformingUSP Class VI certifiedInformation provided by Styrolution |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Techmer ES HiFill® PA6 0201 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Westlake Plastics Absylux® CN-P Acrylonitrile-Butadiene-Styrene (conductive) Carbon-powder-filled conductive material with high strength and stiffness, and relatively high impact strength. This material is easily machined and fabricated into close tolerance finished parts. .. |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Ecomass® 1080ZD92 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Ecomass® 1080ZD93 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
CPC - Vycom SEABOARD™ Supreme DS High density polyethylene (HDPE) Seaboard DS is a high density polyethylene (HDPE) foam core product with a specially formulated skin to add stiffness and Dimensional Stability. This new product from Compression Polymers combines l.. |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Ensinger Tecatron® XP-69 Compression Molded PPS Compound, 35% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Asahi Kasei Thermofil P-20TC-1161 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Asahi Kasei Thermofil P-20TC-5100R 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 49.6 MPa | 7200 psi | ASTM D790 |
Asahi Kasei Thermofil P-40TC-1156 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 49.6 MPa | 7200 psi | |
BCC Products BC 7062-3H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
Flexural Strength | 49.6 MPa | 7200 psi | |
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge cas.. |