Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
PolyOne Maxxam™ FR PP 307 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Quadrant EPP Proteus® O & P Grade, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet) |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Quadrant EPP Proteus® PP, Black Homopolymer Polypropylene (ASTM Product Data Sheet) High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion.. |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Quadrant EPP Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet) High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion.. |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Chesterton ARC BX1 Sliding Wear Compound Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at.. |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Ensinger Tecatron® XP-84 Compression Molded PPS Compound, 30% Graphite Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | <= 33.1 MPa | <= 4800 psi | ASTM D790 |
Arkema Group Solarkote® P-610 Acrylic PVC Capstock, clear, low glossInformation provided by Arkema Group |
|||
Flexural Strength | <= 33.1 MPa | <= 4800 psi | ASTM D790 |
Arkema Group Solarkote® P-600 Acrylic PVC Capstock, clear, high glossInformation provided by Arkema Group |
|||
Flexural Strength | <= 33.1 MPa | <= 4800 psi | ASTM D790 |
Arkema Group Solarkote® P-601 Acrylic PVC Capstock, white, high glossInformation provided by Arkema Group |
|||
Flexural Strength | <= 33.1 MPa | <= 4800 psi | ASTM D790 |
Arkema Group Solarkote® P-611 Acrylic PVC capstock, white, low glossInformation provided by Arkema Group |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |