Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 32.0 MPa | 4640 psi | 2 mm/min; ISO 178 |
Polimeri Europa Edistir RK 5512G Polystyrene UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and to the light
exposure.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | 2 mm/min; ISO 178 |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Flexural Strength | <= 32.0 MPa | <= 4640 psi | ISO 178 |
Polykemi AB POLYelast TPE HJ752 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 32.0 MPa | <= 4640 psi | ISO 178 |
Polykemi AB POLYfill PPC GK8020 Polypropylene Copolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 32.0 MPa | 4640 psi | |
Pyrotek NAD-500 Electrical Insulation Product Cement reinforcement, Inorganic fiber resinApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasket.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | <= 32.0 MPa | <= 4640 psi | ISO 178 |
Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 32.0 MPa | 4640 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EC6400 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
LG Chemical LUCEL ST-550 Ultra High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
Lucent Polymers TPO-30T Thermoplastic Polyolefin, 30% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
Styrolution Polystyrol 485 I GR 2 PS Description: Polystyrol 485 I GR2 is a high-impact grade of polystyrene for extruded sheets with a matt surface.Applications: Sheet, semi finished goods, fat resistant food packaging.Information pro.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
Styrolution PS 485N HIPS Styrolution PS 485N is a high impact grade of polystyrene for extruded sheets with a matte surface.Matte SurfaceUL 94 HBInformation provided by Styrolution |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials R20 C Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials 1st Class Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials 2nd Class Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
Polyplastics Duracon® SX-35 Acetal Co-polymer (POM), Flexible, Lower noise DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EB6400 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Flexural Strength | 32.0 MPa @Temperature 23.0 °C |
4640 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® HD 550 C Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM Test |
BASF Ultramid® 8253 PA6 (Conditioned) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | |
3M Scotchkote™ PR 504 Urethane Pipe Repair Scotchkote Urethane Pipe Repair PR 504 is a special fast curing moisture activated repair bandage for repair bandage for repairs to leaking pipes.Product Features:Easy to apply, requiring no special.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436T30L1 Talc Reinforced |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
Teknor Apex Sinpolene CPP2040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials 3rd Class Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials R20 P Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | 0.1 in/min; ASTM D790 |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |