Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet) Natural and Black |
|||
Flexural Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |
|||
Flexural Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 31.7 MPa | 4600 psi | ASTM D-790 |
CMT Materials REN Shape® 5008 Vacuum Forming Tooling Board REN SHAPE 5008 is a tooling board specifically designed for use in vacuum forming. It is designed for use up to 250°F and is well suited for building vacuum forming molds as well as master models,.. |
|||
Flexural Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene Product CharacteristicsGood impact resistanceConsistent colorabilityEasy processingFood Contact CompliantUL Classification 94HBTypical ApplicationsExtruded SheetSmall AppliancesRefrigeration Accesso.. |
|||
Flexural Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Adell RZ-18 Copolymer Polypropylene, 40% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |