Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 305 MPa @Temperature 23.0 °C |
44200 psi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 305 MPa | 44200 psi | |
Lehmann & Voss LUVOCOM® 3/CF/30/EG Polyamide 6, with carbon fiber, extrusion grade Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Flexural Strength | 305 MPa | 44200 psi | |
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Flexural Strength | 305 MPa | 44200 psi | ISO 178 |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Flexural Strength | 305 MPa | 44200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RE004 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 305 MPa | 44200 psi | ASTM D790 |
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Strength | 305 MPa | 44200 psi | ASTM D790 |
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu.. |
|||
Flexural Strength | 305 MPa | 44200 psi | ASTM-D790 |
Polyram Polytron A35B01 Nylon 66, Chemically Coupled 35% Long Fiber A CHEMICALLY COUPLED 35% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Strength | 305 MPa | 44200 psi | ISO 178 |
Polyram PlusTek PB202G50BK39 Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by NSF/ANSI 61 International.Information provided by Polyram. |
|||
Flexural Strength | 305 MPa | 44200 psi | ASTM-D790 |
Polyram Polytron A35N01 Nylon 66, Chemically Coupled 35% Long Fiber A CHEMICALLY COUPLED 35% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 305 MPa | 44200 psi | |
Lehmann & Voss LUVOCOM® 1-7003 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |