Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 300 MPa | 43500 psi | |
Plastcom SLOVAMID 66 GF 45 PA66, 45% glass fibre FeaturesChemically reinforced with 45% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Plastcom SLOVAMID 66 GF 50 LS PA66, 50% glass fibre, light stability FeaturesChemically reinforced with 50% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry, l.. |
|||
Flexural Strength | 300 MPa | 43500 psi | STN EN ISO 178 |
Plastcom SLOVAMID 66 GF 50 Polyamide 66, 50% Glass Fiber FeaturesChemically reinforced with 50% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1106-7033 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1-1114 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Electrically conductive, suitable for continuous dischar.. |
|||
Flexural Strength | 300 MPa | 43500 psi | 2mm/min; ASTM D790 |
Kingfa PA66-G50 50% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
ICE Al2O3 99.8 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1/CF/15/HS Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1/CF/20/TF/5 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Flexural Strength | 300 MPa | 43500 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® DW-1130 Polyphthalamide (PPA), 30% Glass Fiber Amodel® DW-1130 is a 30% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Flexural Strength | 300 MPa | 43500 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Flexural Strength | 300 MPa | 43500 psi | ASTM D790 |
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu.. |
|||
Flexural Strength | 300 MPa | 43500 psi | ASTM D790 |
Polyram PlusTek PA303G43 Nylon 6.6, 43% Glass Fiber 43% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 300 MPa | 43500 psi | ISO 178 |
Polyram PlusTek RA303G50 Nylon 66 for Injection Molding, 50% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant 50% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
CoorsTek StatSafe™ ADC Static Dissipative Alumina Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffnes.. |
|||
Flexural Strength | >= 300 MPa @Diameter >=100 mm |
>= 43500 psi @Diameter >=3.94 in |
Perpendicular to laminations; IEC 1212-2 4.1 |
Hippe EP GC 21 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relative .. |
|||
Flexural Strength | >= 300 MPa @Diameter >=100 mm |
>= 43500 psi @Diameter >=3.94 in |
Perpendicular to laminations; IEC 1212-2 4.1 |
Hippe EP GC 22 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. High mechanical strength at elevated temperatures. Very good stability of .. |
|||
Flexural Strength | 300 MPa | 43500 psi | 2 mm/min; ISO 178 |
Eurostar Staramide PF00A PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00A is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 300 MPa | 43500 psi | ISO 178 |
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Dry) Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu.. |
|||
Flexural Strength | 300 MPa | 43500 psi | at max force; ISO 178 |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Flexural Strength | 300 MPa | 43500 psi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |