Mechanical Properties Metric English Comments
Flexural Strength 43.7 MPa
6340 psi
ASTM D790
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp
Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren..