Polymer Property : Flexural Strength = 42600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 294 MPa
42600 psi
Conditioned; ASTM D790
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
Flexural Strength 294 MPa
42600 psi
ASTM D790
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Coolant temperature control partsInformation provided by API-Kolon.
Flexural Strength 294 MPa
42600 psi
ISO 178
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod..
Flexural Strength 294 MPa
42600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66
LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare.
Flexural Strength 294 MPa
42600 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA
LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare.
Flexural Strength 294 MPa
42600 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA (Asia Pacific)
LNP* Thermocomp* UF006H is a compound based on Polyphthalamide resin containing Glass Fiber.
Flexural Strength 294 MPa
42600 psi
ASTM D790
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Flexural Strength 294 MPa
42600 psi
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable
Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that..
Flexural Strength 294 MPa
42600 psi
Dry; ASTM D790
Asahi Kasei Leona® 90G33 33% Glass Filled Nylon 66
Enhanced strength and stiffness; with 33% GF. Superior fluidity and appearance.Applications:Automotive parts Information provided by Asahi Kasei