Polymer Property : Flexural Strength = 3900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 26.9 MPa
3900 psi
ASTM D790-95
Multibase Multi-Flex® TPO D 6713
Data provided by Multibase.
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
PolyOne Edgetek® PE-30MC-20TC/000 High Density Polyethylene (HDPE), Talc Filled  (discontinued **)
Description/Features:Mica FilledTalc FilledInformation provided by PolyOne Corporation.
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
Techmer ES HiFill® ABS 0350
Availability: North AmericaFeatures: High DensityForms: PelletsProcessing Method: Extrusion MoldingInformation provided by TP Composites, Inc.
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
Techmer ES Statiblend® 02056 BKN Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc.
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
Techmer ES Statiblend® 02056 Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9111116Information provided by TP Composites, Inc.
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc..
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
Chesterton MRS 5 Metal Rebuilding System
MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we..
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
Techmer ES HiFill® TPU 0445 A
Availability: North AmericaForms: PelletsFeatures: High Density and High Specific GravityInformation provided by TP Composites, Inc.