Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 32.0 MPa | 4640 psi | Y direction, Condition A; ASTM D790 |
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight .. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | 2 mm/min; ISO 178 |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | after 24 hours at ambient temperature |
Pyrotek NAD-11 Structural Insulation Board NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation .. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | |
Pyrotek NAD-500 Electrical Insulation Product Cement reinforcement, Inorganic fiber resinApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasket.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | <= 32.0 MPa | <= 4640 psi | ISO 178 |
Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 32.0 MPa | 4640 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EC6400 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | |
Reliance Industries Polypropylene - Calcium carbonate filled Information provided by Reliance Industries |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
LG Chemical LUCEL ST-550 Ultra High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials R20 C Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
Styrolution Styrolux T SBC Styrolux T is a new developmental, clear and tough styrene-butadiene copolymer (SBC) designed specifically for high performance film extrusion and shrink film applications. Styrolux T has been devel.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MC004 PP (Europe-Africa-Middle East) LNP* Thermocomp* MC004 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials 1st Class Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials 2nd Class Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
Polyplastics Duracon® SX-35 Acetal Co-polymer (POM), Flexible, Lower noise DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EB6400 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Flexural Strength | 32.0 MPa @Temperature 23.0 °C |
4640 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® HD 550 C Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM Test |
BASF Ultramid® 8253 HS PA6 (Conditioned) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | |
3M Scotchkote™ PR 504 Urethane Pipe Repair Scotchkote Urethane Pipe Repair PR 504 is a special fast curing moisture activated repair bandage for repair bandage for repairs to leaking pipes.Product Features:Easy to apply, requiring no special.. |
|||
Flexural Strength | 32.0 MPa | 4640 psi | ASTM D790 |
Teknor Apex Sinpolene CPP2040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati.. |
|||
Flexural Strength | <= 32.0 MPa | <= 4640 psi | ISO 178 |
Polykemi AB POLYfill PP HJ752 UV2 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials 3rd Class Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Flexural Strength | >= 32.0 MPa | >= 4640 psi | |
Sinotek Materials R20 P Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |