Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 310 MPa | 45000 psi | ISO 178 |
PolyOne OnForce™ LFT NN-50LGF/000 HS Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
Oxford Polymers Oxnilon 6-43GF 43% Glass Fiber Filled Nylon 6 for Injection Molding 43% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Strength | 310 MPa | 45000 psi | |
Pyrotek MC-1 Metal Ceramic Thermocouple Protection Tube For casting, MC-1 thermocouple protection tubes are a unique blend of metal and ceramic, exhibiting properties not found solely in either individual material. MC-1 tubes offer high thermal conducti.. |
|||
Flexural Strength | 310 MPa | 45000 psi | ISO 178 |
Nilit FRIANYL B63 GV50 Nylon 6 for injection molding, 50% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 310 MPa | 45000 psi | ISO 178 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA)
(Unverified Data**) Ixef 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1025/9.. |
|||
Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
LNP Stat-Kon® EC-1008 EM BK8-115 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically Conductive, Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Flexural Strength | 310 MPa | 45000 psi | |
Lehmann & Voss LUVOCOM® 20-0791 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Flexural Strength | 310 MPa | 45000 psi | |
Lehmann & Voss LUVOCOM® TPI-8257 Thermoplastic polyimide, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.High-strength and high-stiff parts; lo.. |
|||
Flexural Strength | 310 MPa | 45000 psi | |
GBC Grade 85 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Flexural Strength | 310 MPa | 45000 psi | 5 mm/min; ISO 178 |
Gromax BFG45-AS00N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 310 MPa | 45000 psi | 5 mm/min; ISO 178 |
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 310 MPa | 45000 psi | ISO 178 |
Solvay Technyl® A218V43 43% Glass Filled, Heat Stabilized Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Strength | 310 MPa | 45000 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing 45% Glass Fiber. |
|||
Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RX05491 PA 66 LNP* Thermocomp* RX05491 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
Techmer ES Electrablend® PA6 CF30 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: Conductive Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 310 MPa | 45000 psi | ISO 178-93 |
Wellman Wellamid® GFX1717-N1 43% Glass Fiber Reinforced, Silicone Lubricated Nylon 66 Description: Glass Fiber Reinforced, Silicone Lubricated Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 310 MPa | 45000 psi | 2 mm/min; ISO 178 |
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar. |
|||
Flexural Strength | 310 MPa | 45000 psi | Elastic Limit in Bending, across direction of rolling |
CLAL-MSX CUPROROR® TL5 Spring, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
Ashley Polymers Ashlene® 528L-50G Nylon 66, 50% Glass Reinforced A general purpose 50% glass reinforced Nylon 66 resin.Data provided by the manufacturer |
|||
Flexural Strength | 310 MPa | 45000 psi | |
Anderman Ceramics EA96 Sintered Alumina, 96% High strength alumina (96%) available pink or white. Available in many shapes and sizes.Information provided by Anderman Ceramics. |
|||
Flexural Strength | 310 MPa | 45000 psi | |
Anderman Ceramics EA995 Sintered Alumina, 99.5% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Flexural Strength | 310 MPa | 45000 psi | 45° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
LNP Thermocomp® UF-1008 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |