Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 30.0 MPa | 4350 psi | |
Plastcom SLOVALEN PC 78 FRT 5 PP, glass fibre, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Flexural Strength | 30.0 - 40.0 MPa | 4350 - 5800 psi | ASTM D790-03 |
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Radici Radilon® SLVHPL128 (dry) Nylon 6 Plasticized for improved flexibilityInformation provided by Radici group. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1221 High gloss PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1249 Sanitary, mix color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Strength | <= 30.0 MPa | <= 4350 psi | ISO 178 |
Polykemi AB POLYfill PP EVR8025H UV Polypropylene/EDPM, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 30.0 MPa @Temperature 22.0 °C |
4350 psi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Lucent Polymers TPO-20T Thermoplastic Polyolefin, 20% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Kostat BK-STAT R048BK PS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Kostat E-3007J Conductive PS Compound KOSTAT E-3007J is a conductive thermoplastic compound based on impact modified polystyrene and a special conductive carbon black.KOSTAT E-3007J is not dependant on atmospheric conditions.Special Fea.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Solvay TECHNYL® C 402 M PA6, Conditioned Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high .. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Solvay TECHNYL® eXten D 458P PA6.10, DRY Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, .. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | |
SPS Guang Zhou SAMATâ„¢ 666(f1) Flame-retarded Polypropylene Characteristic: Flame retardance, weather resistance, good mechanical propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Borealis Daplen™ EE158AI Polypropylene TPO Compound Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Unitika A1030TF PA6, Conditioned Lubricating nylonInformation provided by Unitika Ltd. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | GB/9341 |
Zhejiang Juner JEPP2007 PP For Automotive Parts Applications: Inner Decorate PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Aclo Accucomp Polypropylene CPO402V Automotive Approved Copolymer Extrusion Grade |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Flexural Strength | 30.0 MPa @Temperature 65.0 °C |
4350 psi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM Test |
BASF Ultramid® 8350 HS PA6 (Conditioned) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436M20L Mica Reinforced |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Polyplastic Armlen® PP MF 40-2HS Polypropylene, 40% Mineral Filled Impact modified, injection moldingInformation provided by PolyPlastic Group. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
BASF Nypel® 2351 HS BK PA6 (Dry) Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |