Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 203 MPa | 29500 psi | ASTM D790 |
Oxford Polymers PEI -20GF-Natural PEI, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristic.. |
|||
Flexural Strength | 203 MPa | 29500 psi | ASTM D790 |
Techmer ES HiFill® PEI GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 203 MPa | 29500 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF30 ML5 HS 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and Heat Stabiliz.. |
|||
Flexural Strength | 203 MPa | 29500 psi | ASTM D790 |
Teknor Apex Chemlon® 233 GI Nylon 6, 33% Glass Fiber Reinforced Features: High Impact, 33% Glass Reinforced; Highly toughened compound exhibiting strength and rigidity; Good Creep Resistance; Good Stiffness; Good Toughness; Impact Modified Processing Method: Inj.. |
|||
Flexural Strength | 203 MPa | 29500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM1 HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Strength | 203 MPa | 29500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM1 L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedInformatio.. |
|||
Flexural Strength | 203 MPa | 29500 psi | ASTM D790 |
Ensinger Tecapeek® XP-103 Compression Molded PEEK Compound, 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 203 MPa | 29500 psi | ASTM D790 |
Teknor Apex Chemlon® 109-33 GH Nylon 66, 33% Glass Fiber Filled Notes: High-Impact; Reinforced with 33% Glass Fibers; Highly toughened compound exhibiting strength and rigidity Features: Good Creep Resistance; Good Stiffness; High Strength; Good Impact Resistanc.. |