Polymer Property : Flexural Strength = 28000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 170 - 193 MPa
24700 - 28000 psi
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound
BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe..
Flexural Strength 170 - 193 MPa
24700 - 28000 psi
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound
BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos..
Flexural Strength 179 - 193 MPa
26000 - 28000 psi
Bulk Molding Compounds BMC 1410 Electrical Grade
BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally..
Flexural Strength 165 - 193 MPa
24000 - 28000 psi
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound
BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression..