Polymer Property : Flexural Strength = 28.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (Cond)
Information provided by Ravago.
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (Cond)
Information provided by Ravago.
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Techmer ES HiFill FR® CONC HDPE FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Techmer ES HiFill FR® HDPE 8904 FR UV GY
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceAppearance: GrayInformation provided by TP Composites, Inc.
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Techmer ES HiFill FR® HDPE E FR
Availability: North AmericaForms: PelletsFeatures: Flame Retardant Processing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Techmer ES HiFill FR® HDPE FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Techmer ES Statiblend® HIPS E
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveAppearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Techmer ES Plastiblend® LDPE E FR V-2
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Americas Styrenics EB6755 High Impact Polystyrene
Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa..