Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 27.4 MPa | 3970 psi | 2mm Deflection; ASTM D790 |
Reliance Industries PVAXX H65 The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie.. |