Mechanical Properties Metric English Comments
Flexural Strength 184 MPa
26700 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific)
LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 184 MPa
26700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON DEL36 PC
LNP* STAT-KON* DEL36 is a compound based on Polycarbonate resin containing 30% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Wear Resistant.
Flexural Strength 184 MPa
26700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon EE002ER PEI (Europe-Africa-Middle East)
LNP* Lubricomp* EFP36G is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.This data wa..
Flexural Strength 184 MPa
26700 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON WE002 PBT
LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 184 MPa
26700 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON WE002 PBT (Asia Pacific)
LNP STAT-KON* WE002 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 184 MPa
26700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA6.12
LNP* THERMOCOMP* IF004 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber.
Flexural Strength 184 MPa
26700 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DE003P PC
LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing.
Flexural Strength 184 MPa
26700 psi
ISO 178
SABIC Innovative Plastics LNP VERTON MX02795 PP
LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural.
Flexural Strength 184 MPa
26700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66
Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region.
Flexural Strength 184 MPa
26700 psi
ASTM D570
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer  (discontinued **)