Mechanical Properties Metric English Comments
Flexural Strength 182 MPa
26400 psi
ASTM D790
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East)
LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Flexural Strength 182 MPa
26400 psi
ASTM D790
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66
LNP* KONDUIT* RTF2B is a compound based on Nylon 66 resin containing 10% Glass Fiber, 55% Thermal Filler. Added features of this material include: Thermally Conductive.
Flexural Strength 182 MPa
26400 psi
ASTM D790
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific)
LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Flexural Strength 182 MPa
26400 psi
ASTM D790
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable..
Flexural Strength >= 182 MPa
>= 26400 psi
MarkeTech Repton 125 Aluminum Oxide
Brand 125 features: High Purity Standard.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when t..
Flexural Strength 182 MPa

@Temperature 22.0 °C
26400 psi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP
SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac..
Flexural Strength 182 MPa
26400 psi
1.3 mm/min; ASTM D790
Lavergne VYPET 2130 Polyester Alloy Resin, 30% Fiberglass Reinforced
Vypet 2130 is a 30% fiberglass reinforced, toughened Modified PBT injection molding compound designed for structural and electrical applications.Features: High temperature performances; Excellent di..
Flexural Strength 182 MPa
26400 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT
LNP LUBRICOMP* WFL34H is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Healthcare.
Flexural Strength 182 MPa
26400 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON AE006 ABS
LNP* STAT-KON* AE006 is a compound based on ABS containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Flexural Strength 182 MPa
26400 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific)
LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber.
Flexural Strength 182 MPa
26400 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DE003ER PC
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive.
Flexural Strength 182 MPa
26400 psi
ASTM D 790
SABIC Innovative Plastics Valox® 553M PBT+PC (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Strength 182 MPa
26400 psi
ASTM D790
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to..
Flexural Strength 182 MPa
26400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V4860HR PBT
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Flexural Strength 182 MPa
26400 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES
LNP THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing 20% Glass Fiber.
Flexural Strength 182 MPa
26400 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Asia Pacific)
LNP* THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber.
Flexural Strength 182 MPa
26400 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific)
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Flexural Strength 182 MPa
26400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific)
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Flexural Strength 182 MPa
26400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East)
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Flexural Strength 182 MPa
26400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT
LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber.
Flexural Strength 182 MPa
26400 psi
ASTM D790
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Flexural Strength 182 MPa
26400 psi
ASTM D790
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Flexural Strength 182 MPa
26400 psi
ASTM D790
Plenco 6401 Phenolic, Briquette, Transfer Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Flexural Strength 182 MPa
26400 psi
ASTM D790
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Flexural Strength 182 MPa
26400 psi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced
Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol..
Flexural Strength 182 MPa
26400 psi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced
Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol..
Flexural Strength 182 MPa
26400 psi
ASTM D790
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Flexural Strength 182 MPa
26400 psi
ASTM D790
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Flexural Strength 182 MPa
26400 psi
ASTM D790
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Flexural Strength 182 MPa
26400 psi
ISO 178
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject..