Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 220 - 230 MPa | 31900 - 33400 psi | ISO 178 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Flexural Strength | 220 - 230 MPa | 31900 - 33400 psi | Higher values are for NT and BK324.; ISO 178 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This .. |