Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 23.4 MPa | 3400 psi | ASTM D790 |
Multibase Multi-Pro® 0710 C Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Strength | 23.4 MPa | 3400 psi | ASTM D790 |
Quadrant EPP Durapro® Truck Liners (ASTM Product Data Sheet) |
|||
Flexural Strength | 23.4 MPa | 3400 psi | |
UCAR Carbon UCAR® CSX Extruded Graphite Densified prior to graphitization, Grade CSX is an extruded graphite, higher in strength and lower in permeability than CS. It is a material for applications requiring higher densities, better mecha.. |
|||
Flexural Strength | 23.4 MPa | 3400 psi | ASTM D790 |
BCC Products DP-11-88 Urethane Adhesive DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions .. |
|||
Flexural Strength | 23.4 MPa | 3390 psi | 20 x 40 mm |
CeramTec 447 Cordierite, 2MgO•Al2O3•5SiO2 Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |