Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2.60 MPa | 377 psi | 1% Sec; ASTM D-790-92 |
Multibase Multi-Flex® TPE A 8502 EXCEL GREY Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Krato.. |
|||
Flexural Strength | 2.60 MPa | 377 psi | 1% Sec; ASTM D-790-92 |
Multibase Multi-Flex® TPE A 8592 MEDIUM TAUPE Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Krato.. |
|||
Flexural Strength | 2.60 MPa | 377 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU) Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersi.. |
|||
Flexural Strength | 2.60 MPa | 377 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU) Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersin.. |
|||
Flexural Strength | 2.60 MPa | 377 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU)
(Unverified Data**) Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing.. |
|||
Flexural Strength | 2.60 MPa | 377 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU)
(Unverified Data**) Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing .. |